ASTM E316 – Standard Test Method for Determination of Iron in Manganese Ores by Hydrogen Sulfide Reduction-Dichromate Titrimetry
1.1 This test method covers the determination of iron in manganese ore in the range from 2 % to 20 %.
Note 1:As used in this test method (except as related to the term relative standard deviation), “percent” or “%” refers to mass fraction (wt/wt) of the form 1g/100g.